Metallic inlet repair fails when it gets treated like cosmetic metalwork. I approach it as precision recovery of geometry, sealing, stiffness, and decibel behavior, because a repaired inlet that looks good but whistles, leaks, or distorts under load is still a bad repair. What follows is the full workflow I use to bring damaged metallic inlet assemblies back to service with controlled surface re-profiling and measurable acoustic recovery.
What You’ll Need Before Starting a Metallic Inlet Repair
A serious repair starts long before heat, filler, or abrasives touch the part. I set the job up as a controlled restoration process, with metrology, inspection discipline, and hard acceptance limits already in place.
Required tools, metrology, and inspection equipment
I never begin advanced inlet work with hand tools alone. At minimum, I want a borescope for internal passages, a profilometer for surface roughness, precision straightedges, radius gauges, contour gauges, digital calipers, depth mics, and an ultrasonic thickness gauge. If the inlet is thin-wall aluminum, I add a dial-indicator setup for runout and flange movement, because thin housings move fast when heat enters the equation.
For geometry control, specialized jigs matter. I use rigid fixture plates, concentricity mandrels, split-clamp ring supports, flange-backup plates, and adjustable locator pins to hold aluminum inlets in their true installed relationship. Soft-jaw supports help prevent witness marks, but the real value is positional repeatability. A housing held in a crude bench vise never keeps its intended profile.
Inspection gear needs to cover both visible and hidden damage. White light, magnification, dye penetrant kits, and thickness mapping are standard. For premium work, I prefer digital contour capture, because 3D scan-driven rebuilds remove guesswork from re-profiling complex curves.
Acoustic verification belongs on the bench plan from the start, not at the end as an afterthought. I use calibrated decibel meters, vibration sensors, and, where applicable, narrow-band frequency analysis to compare post-repair behavior against baseline records or matched-service components. That discipline lines up with the broader reality that fleet acoustic recovery depends on measurement, not opinion, a point reinforced in post-overhaul sound validation practices.
Repair materials and consumables
Consumables have to match the service environment and substrate. I keep filler alloys and weld wire selected by parent metal chemistry, not convenience. For aluminum inlet structures, that usually means tightly matched TIG filler and a documented heat-input plan. For localized contour restoration in non-primary zones, engineered metal-loaded compounds and bonded rebuild materials earn their place, but only after the damage has been fully stabilized.
I also stage abrasives in a controlled sequence, from coating removal media to fine blending discs and polishing sheets for final finish correction. Masking materials, anti-spatter barriers, corrosion inhibitors, surface activators, primers, compatible topcoats, and sealing products all need to be in reach before the first cut. Stopping mid-repair to substitute an unqualified product is how contamination creeps in.
Safety, isolation, and documentation requirements
Before touching the inlet, I lock out connected systems, isolate stored pressure, and control thermal exposure. If the assembly lives near engine, bleed-air, or electrical interfaces, I treat adjacent hardware as contamination-sensitive and service-critical. That means protected transport, capped passages, clean benches, and no open abrasive work near exposed acoustic media or sealing faces.
Documentation is just as important as tooling. I work from OEM limits, approved repair manuals, fleet deviations, prior defect history, and serialized part records. Traceability has to capture what was found, what was removed, what material was added, what inspection was repeated, and how the repaired shape was verified. On a service-critical inlet, undocumented work is functionally the same as unapproved work.
Understand When Metallic Inlet Repair Is Appropriate
Not every damaged inlet deserves repair. Some parts are recoverable with excellent results. Others are scrap the moment the true extent of distortion becomes clear.
Repairable versus non-repairable damage
I classify localized erosion, shallow gouging, discrete pitting, limited crack initiation, flange nicking, and modest profile loss as repairable, assuming thickness and geometry stay inside the approved envelope. Edge damage is often recoverable if sound metal remains behind the defect and the rebuild does not push the section into excessive heat exposure.
I reject widespread distortion, deep through-section fractures in highly loaded zones, extensive corrosion undermining multiple interfaces, and any housing that has drifted out of tolerance across its mounting pattern or bore alignment. Once the base structure stops holding datum reliably, repair turns into guesswork. I do not gamble on mission-critical geometry.
How repair scope affects acoustic and structural performance
Small defects change more than appearance. A slight depression or abrupt blend line can trip airflow, create local turbulence, alter pressure behavior, and shift tonal noise. A rough rebuilt zone can also affect damping response by changing how the surface interacts with adjacent acoustic treatments and pressure pulses. That is why I often cross-check surface recovery against laminar-flow acoustic behavior in nacelle systems.
Structurally, every notch, heat tint zone, or partially excavated crack becomes a fatigue story waiting to unfold. Aerospace and composite repair literature keeps repeating the same lesson: visual damage rarely captures the real defect field, and non-destructive inspection matters because hidden propagation changes the repair decision completely. Metallic inlet work follows the same rule.
Step 1: Review Service Data and Establish Repair Limits
I define the repair on paper before I define it on metal. That prevents scope creep, unnecessary material removal, and false confidence.
Collect drawings, tolerance bands, and past repair history
- I gather service manuals, sectional drawings, contour references, and material callouts for the exact inlet configuration.
- I pull prior repair records, repetitive discrepancy logs, and any recurring vibration or noise findings tied to the same part number.
- I compare current damage location against known fleet failure patterns, especially erosion bands, bracket-induced cracking, and flange fretting.
Past history matters more than many shops admit. If the same area has already been built up twice, I treat the next repair as a structural review, not routine rework. If decibel complaints followed the previous restoration, I tighten finish and contour controls before moving further.
Define pass/fail criteria before disassembly
- I write the maximum permissible material loss, minimum remaining thickness, and allowable crack extent.
- I set surface finish targets, profile tolerances, flange flatness limits, and alignment tolerances.
- I define leak-tightness expectations and acceptable acoustic recovery bands against baseline readings.
- I identify replacement triggers so the job does not drift into unauthorized salvage.
This step saves time later. It also prevents the common trap of building material back onto a part that was already beyond dimensional recovery.
Step 2: Remove the Inlet and Prepare the Work Area
Bad removal practices create fresh damage, and fresh damage hides inside old damage. I keep removal slow, supported, and documented.
Isolate connected systems and remove surrounding hardware
- I isolate all connected mechanical, electrical, pneumatic, and environmental interfaces.
- I remove fasteners in sequence, supporting the housing so the damaged zone never carries the extraction load.
- I remove seals, liners, brackets, and adjacent components with dedicated trays and identification tags.
- I cap internal passages immediately to prevent abrasive, solvent, or shop debris entry.
When the inlet sits beside acoustic treatment, I treat that material as fragile and contamination-sensitive. For assemblies with adjacent perforated skins or liners, the handling logic follows the same discipline I apply in high-speed perforated-face repairs.
Clean, label, and fixture the component for repair
- I perform a preliminary non-destructive cleaning to remove grime, oil, and loose corrosion product.
- I mark orientation, datum references, and defect zones before deeper stripping removes visual clues.
- I create a damage map directly on photos and inspection sheets.
- I fixture the component on a rigid support that simulates installed geometry.
This is where specialized jigs earn their keep again. Aluminum inlets distort if they are held by one flange ear or a narrow clamp line. I use full-contact support rings, locator bosses, contour saddles, and restraint bridges that spread load across stable sections while leaving the repair zone accessible. A proper jig does two jobs at once: it preserves shape during measurement and resists movement during localized heating.
Step 3: Perform a Detailed Damage Assessment
The visible scar is only the headline. The real condition lives in the surrounding material, wall thickness, and interface relationships.
Conduct visual, dimensional, and non-destructive inspection
- I begin with white-light visual inspection and magnification, documenting all visible pits, gouges, cracks, and coating failures.
- I run dye penetrant across suspect edges, weld toes, and transition zones.
- I check remaining wall thickness ultrasonically, especially near corrosion fields and eroded lips.
- I measure runout, flatness, bore relationship, and contour deviation from baseline templates or scan data.
- I inspect internal passages with a borescope to catch backside cracking or hidden debris traps.
That sequence tells me whether the damage is isolated or systemic. If the contour loss is broad but shallow, rebuild and finish work make sense. If the defect has migrated into bolt patterns, liner seats, or structural corners, I reassess repairability immediately.
Map damage zones by function
- I separate primary structural damage from surface-only loss.
- I isolate sealing-face defects from aerodynamic contour defects.
- I flag acoustically sensitive surfaces that require tighter blending and finish control.
- I mark no-go areas where heat, grinding, or compound use is restricted.
I like this functional map because it prevents a lazy one-method repair. A crack at a bracket root does not get treated the same way as shallow contour erosion near an inlet lip. Different zones demand different restoration logic.
Step 4: Select the Best Repair Method for the Damage Type
Method selection drives the outcome. A good technician with the wrong process still gets a poor repair.
When to use weld build-up or micro-TIG repair
- I choose weld build-up or micro-TIG when the defect affects strength, crack continuity, or edge integrity.
- I use it for localized material replacement, crack arrest after full excavation, and structurally meaningful lip rebuilds.
- I keep bead size small and heat input controlled, especially on thin aluminum sections.
This is the right answer when metallurgical continuity matters. It is not the right answer when the area is so thin or distortion-sensitive that the cure becomes worse than the defect.
When to use brazing or low-heat restoration
- I use brazing or other low-heat methods for thin sections, localized seepage paths, and non-primary load regions.
- I choose it when distortion risk outweighs the need for full structural fusion.
- I verify compatibility with downstream coatings, corrosion exposure, and service temperature before approval.
The benefit is lower thermal damage. The catch is lower structural margin, so I keep this method out of primary recovery zones.
When additive rebuild or laser deposition is justified
- I select additive rebuild for high-value housings with precise contour loss and limited tolerance for bulk heat.
- I use it when replacement lead time or asset value justifies premium restoration.
- I pair it with scan-based reverse engineering and controlled finish machining.
This is where turbine remanufacturing offers a valuable lesson. Laser metal deposition creates far less distortion than conventional arc repair on difficult alloys, and the same logic applies when preserving inlet geometry matters more than low upfront process cost.
When bonded or polymer-metal repairs are acceptable
- I approve bonded or metal-filled repairs only for non-critical contour recovery, corrosion stabilization, or surface sealing in approved zones.
- I require complete substrate preparation and firm boundaries around service load and temperature exposure.
- I prohibit these materials from replacing true structural restoration where crack growth or load transfer is involved.
Used correctly, they are practical. Used as a shortcut, they are a liability.
Step 5: Strip Coatings, Remove Damage, and Prepare the Substrate
Preparation determines bond quality, weld quality, and repair life. Poor prep ruins even the best restoration method.
Remove coatings, oxides, and contamination without overcutting
- I strip coatings with the least aggressive method that fully exposes sound substrate.
- I use controlled abrasive blasting, approved chemical stripping, solvent cleaning, and oxide removal matched to the alloy.
- I protect untouched parent metal and all no-damage interfaces with masking and shields.
I never chase cosmetic cleanliness by eroding good metal. The goal is exposed, stable substrate, not a larger repair.
Excavate cracks, pits, and damaged material to a stable geometry
- I grind out defects until penetrant and visual evidence show sound metal.
- I radius cavity transitions to remove stress risers.
- I stop-drill crack tips only where the approved data permits it.
- I shape the cavity for complete fill and later contour control.
The excavation geometry matters. Narrow, dirty grooves trap oxide and make fusion erratic. Broad, controlled cavities fill cleaner and finish better.
Prepare edges and thermal conditions for rebuild
- I bevel edges where weld access requires it.
- I set preheat only when the alloy and thickness call for it.
- I monitor interpass temperature tightly.
- I thermal-balance the setup with chill bars, backing plates, and staged sequencing.
Low-distortion heat practice is not optional on aluminum inlet work. I borrow heavily from thermal-control methods used in adjacent housing repairs because the same principles keep thin metallic structures stable.
Step 6: Rebuild Lost Material Using the Chosen Restoration Technique
This is the point where patience pays off. Fast deposition creates long finishing hours and unstable geometry.
Apply weld, braze, or additive layers in controlled passes
- I deposit in thin, deliberate passes instead of one oversized fill.
- I place beads or layers to support the final contour rather than bury it under excess material.
- I allow cooling intervals that keep the repair local.
- I inspect between passes for wet-out, fusion quality, and edge integrity.
On premium jobs, I intentionally underbuild by a controlled allowance that matches final machining stock. That keeps post-process grinding shallow and predictable.
Manage distortion and residual stress during the rebuild
- I use fixture restraint that holds datum without forcing artificial stress into the housing.
- I stagger deposition so heat does not stack in one direction.
- I add chill blocks or heat sinks near vulnerable sections.
- I measure flange movement and bore relationship during the rebuild, not only after it.
Advanced remanufacturing research on turbine components shows that hybrid scan, deposit, and machine workflows improve form control, with targets as tight as Ra < 1.6 μm and sub-50 μm form accuracy for aerodynamic surfaces. Metallic inlet work does not always require that level, but the mindset is exactly right.
Protect adjacent sealing and acoustic interfaces
- I mask flange faces, gasket lands, liner seats, and mating edges before deposition starts.
- I shield adjacent acoustic surfaces from spatter, abrasive contamination, and heat tint.
- I inspect interface boundaries after each repair phase.
I never accept a successful rebuild that damages the sealing or acoustic features around it. That is trading one defect for another.
Step 7: Machine, Grind, and Re-profile the Surface to Original Geometry
Surface re-profiling is where the repair becomes real. Until this step is finished and verified, the job is only a material build-up.
Re-establish datum points and reference contours
- I re-reference the part to original datums before removing any excess material.
- I use templates, contour gauges, scan overlays, CMM data, or known-section measurements to guide shaping.
- I verify the setup in the fixture before any finish pass.
I do not shape by eye. On simple lips, templates work well. On compound aluminum inlet curves, I prefer digital overlays and jig-mounted sweep gauges. Those tools maintain repeatable geometry and prevent the common error of chasing smoothness while losing the designed line.
Blend repaired zones into surrounding parent metal
- I remove excess material in stages, switching from machining or coarse grinding to draw-filing and controlled blending.
- I feather transitions wide enough to avoid abrupt slope changes.
- I preserve parent metal thickness instead of grinding everything flat.
- I continuously compare the repaired zone against the untouched surrounding contour.
A smooth-looking patch is not necessarily an aerodynamic patch. Blend shape, transition length, and edge continuity all affect airflow and sound. For inlet structures that sit near broader acoustic systems, the same principle shows up in panel-level decibel restoration work.
Achieve the required surface finish and profile tolerance
- I finish to the specified roughness, radius, and profile tolerance for that inlet zone.
- I verify surface roughness with a profilometer instead of relying on visual appearance.
- I check edge breaks, local waviness, and contour repeatability across the repair boundary.
This is also where I make the final call on acoustic readiness. Even if dimensions pass, a rough or uneven blend can still degrade tonal performance.
Step 8: Restore Sealing Surfaces, Interfaces, and Protective Layers
A repaired contour still fails in service if the assembly leaks, corrodes, or loses interface pressure.
Repair flange faces, gasket lands, and connector interfaces
- I inspect flange flatness and gasket land continuity after surface restoration.
- I lap or resurface faces as needed to recover even sealing pressure.
- I correct bolt-hole distortion, replace inserts where approved, and verify interface spacing.
- I dry-fit mating components before coating application.
This is where many inlet repairs go sideways. The rebuilt contour looks excellent, but the flange face took heat movement and nobody caught it until reinstallation.
Reapply corrosion protection and compatible coatings
- I prepare the restored area to the coating system specification.
- I apply conversion coating, primer, metallic protection, or topcoat compatible with the substrate and service environment.
- I keep coating thickness off critical fits, bores, and sealing lands unless the specification allows it.
Long-term durability depends on this step, especially in salt, moisture, or chemical exposure. For harsh fleet service, I follow the same discipline used in corrosion prevention programs for inlet and nacelle structures.
Step 9: Verify Structural Integrity and Dimensional Accuracy
I treat inspection as the real finish line. If the part has not been proven, it is not repaired.
Repeat NDT and final dimensional inspection
- I repeat dye penetrant on repaired and adjacent heat-affected zones.
- I confirm final wall thickness in all critical areas.
- I check contour recovery, flatness, bore relation, and mating-surface quality against documented limits.
- I inspect coating boundaries and restored edges for defects introduced during finishing.
This second inspection often catches what shop enthusiasm misses, especially tiny toe-line indications or edge undercut after aggressive blending.
Check tolerance stack-up and installation readiness
- I verify hole alignment, flange parallelism, interface spacing, and fastener seating.
- I confirm the part installs without forced alignment.
- I review all recorded dimensions as a system, not as isolated values.
Tolerance stack-up is where acceptable individual numbers can still add up to a bad assembly. I want the part to fit naturally, not be pulled into place by bolts.
Step 10: Validate Acoustic, Flow, and Environmental Performance
This is the section that separates advanced restoration from metal cosmetic work. Structural recovery has to translate into operating performance.
Perform leak, pressure, and sealing checks
- I run leak checks using pressure decay, low-pressure air verification, or approved water-ingress methods.
- I inspect gasket compression witness patterns and sealing continuity.
- I confirm dust and moisture exclusion if the inlet serves an environmental barrier function.
Heavy-duty inlet applications increasingly serve harsh sealed environments, including watertight and dusttight inlet segments, so post-repair sealing performance is not negotiable.
Measure vibration, resonance, and decibel response
- I compare post-repair sound levels against baseline, matched units, or historical service records.
- I monitor vibration amplitude and resonance behavior during operating-condition checks.
- I identify narrow-band noise changes that suggest contour or stiffness issues.
If a repaired inlet passes geometry but fails sound response, I do not call it close enough. For fleets where noise margins matter, repair quality has to align with broader aircraft noise control outcomes.
Confirm airflow or passage uniformity where applicable
- I inspect flow path continuity visually and dimensionally.
- I verify bore alignment and passage symmetry.
- I assess repaired zones for abrupt changes that drive pressure loss or unstable flow.
A simple smoke or low-pressure flow visualization check can reveal a surprisingly bad blend line. Useful. Fast. Worth doing.
Step 11: Reinstall the Inlet and Conduct a Controlled Return-to-Service
The repair is still vulnerable during reinstallation. Mishandled torque or poor alignment can undo hours of controlled restoration.
Reassemble with correct torque, sealing, and alignment practices
- I replace seals and gaskets with approved parts.
- I inspect fasteners, threads, and inserts before installation.
- I torque in sequence with alignment checks at each stage.
- I confirm the repaired area remains unloaded by assembly mismatch.
I never use fasteners to force alignment. If the part does not settle correctly, I stop and recheck the interface condition.
Run post-installation checks and short-interval monitoring
- I perform a first-run inspection after initial operation.
- I review thermal cycling effects, leakage signs, and fastener stability.
- I trend noise and vibration over a short follow-up interval.
- I reinspect the repaired zone before returning the component to normal maintenance intervals.
Short-interval monitoring catches movement early, before a small post-repair shift turns into a repeat event.
Advanced Techniques That Improve Repair Quality
Good repairs restore service. Premium repairs restore service predictably, repeatedly, and with less rework.
Using digital contour mapping for precision surface re-profiling
I rely on 3D scanning and digital overlays whenever the inlet shape is compound, thin, or acoustically sensitive. In turbine remanufacturing, scan systems such as the EinScan Pro 2X have been used to capture worn geometry at 0.04 mm accuracy, and that level of fidelity changes how confidently I can rebuild aluminum inlet contours. Once the scan exists, I can compare every stage of grinding and machining against the intended line instead of judging smoothness by feel.
Applying low-distortion heat management strategies
Chill blocks, localized backing bars, pulse-controlled deposition, asymmetric pass sequencing, and carefully limited preheat all reduce dimensional drift. I also prefer fixtures that support the housing naturally rather than overconstrain it. Overclamping hides movement until the part is released, then the whole geometry walks.
Borrowing additive remanufacturing principles from turbine repair
High-value turbine repairs have used laser deposition since 1996, largely because replacing precision hot-section hardware is expensive and slow. The same economic logic applies to complex metallic inlets when replacement cost, lead time, or fleet availability becomes painful. The lesson I take from turbine work is simple: scan first, add material only where needed, machine minimally, and verify everything.
Common Mistakes to Avoid During Metallic Inlet Repair
Most failed repairs are predictable. The warning signs show up early.
Overbuilding the repair and grinding back too aggressively
Too much fill means too much heat, too much cleanup, and too much opportunity to thin good parent metal while blending. I build only the stock I need. Then I finish only the stock I planned to remove.
Ignoring hidden crack propagation or substrate contamination
A bright surface can still hide oil, oxide, or branching crack paths. I have seen clean-looking repairs fail because the excavation stopped when the defect looked gone instead of when inspection proved it was gone. That is not a finishing issue. That is a process failure.
Treating re-profiling as cosmetic instead of functional
Contour shape drives sealing, airflow, stiffness, and sound behavior. If re-profiling gets treated like polishing, the inlet may pass a quick glance and still fail in service.
Troubleshooting Metallic Inlet Repair Problems
Problems during restoration usually point back to prep, heat control, or geometry control. I diagnose them in that order.
The rebuilt area won’t bond, wet out, or fuse properly
Contamination is the first suspect, followed by oxide retention, filler mismatch, poor cavity shape, or incorrect heat input. I strip back to clean metal, reprepare the cavity, confirm alloy compatibility, and reset the process window. If a bonded compound is involved, I also check substrate roughness and cure conditions because poor surface energy kills adhesion fast.
The housing distorts after welding or material deposition
That points to excessive local heat, poor sequence planning, overconstraint in the fixture, or an unsupported thin section. I map the distortion against original datums, relieve the setup if needed, and correct shape before final finishing. If the movement is recurring, I change pass distribution and add broader support or chill control.
Surface profile passes dimensional checks but fails acoustic targets
This happens when the repaired surface is dimensionally right in a coarse sense but wrong in a functional sense. Local waviness, roughness, voids under a bonded layer, and abrupt blend transitions can all change noise output. I revisit the surface with tighter roughness measurement, contour sampling, and resonance review. In acoustically sensitive assemblies, appearance is a poor predictor of sound quality.
Sealing performance drops after reinstallation
I check flange flatness, coating buildup on gasket lands, misaligned fasteners, wrong gasket compression, and torque sequence errors. Many sealing failures are installation-induced, not repair-induced. But if the flange moved during restoration and nobody requalified it, the repair process owns the failure.
Expected Results After a Successful Repair
A successful repair is measurable. I do not define success by appearance alone.
Structural and dimensional outcomes to expect
The final part should show clean NDT results, restored wall condition, stable datums, correct interface spacing, acceptable flange flatness, and contour recovery inside the defined tolerance band. Installation should occur without forced alignment, and the restored area should carry service load without visible movement or distress.
Acoustic and operational performance benchmarks
The repaired inlet should return to stable dampening behavior, avoid turbulence-related tonal penalties, maintain sealing under operating conditions, and show no unusual vibration response. Left untreated, damage in these areas tends to worsen service life and noise behavior. Proper restoration reverses that trend and gives the component a predictable maintenance future.
Next Steps: Build a Repeatable Metallic Inlet Repair Standard
One good repair helps one part. A documented standard improves the whole fleet.
Create repair decision trees for recurring inlet damage
I classify repeat defects by location, severity, substrate, and service effect, then assign approved methods, escalation triggers, and mandatory replacement points. That turns tribal knowledge into a usable decision path. It also keeps one shop shift from improvising where another shift would reject the part.
Track repair outcomes to improve future restorations
I log distortion rates, material removal depth, chosen repair process, coating performance, leak-check results, decibel findings, and repeat-failure intervals. Those records show which methods actually hold up. Over time, the repair standard gets tighter, faster, and far more defensible.
Frequently Asked Questions
How much damage is too much for metallic inlet repair?
Damage is too extensive once the inlet loses reliable datum control, minimum wall thickness, flange alignment, or crack containment within approved limits. Widespread distortion and deep structural fracture are replacement conditions, not repair conditions.
Is welding always the best option for metallic inlet repair?
No. Welding is the best option when structural recovery and metallurgical continuity are required. Thin sections, non-primary zones, and distortion-sensitive areas often respond better to brazing, additive rebuild, or approved bonded contour restoration.
Why does surface re-profiling matter so much after material rebuild?
Because the inlet does not serve on strength alone. Final contour affects airflow behavior, sealing pressure, vibration response, and decibel output. A badly blended repair can pass a casual inspection and still perform poorly.
What tools keep aluminum inlet geometry stable during repair?
I rely on fixture plates, concentricity mandrels, contour saddles, split support rings, flange backup plates, locator pins, chill blocks, and sweep gauges. Those jigs keep thin aluminum sections from sagging, twisting, or springing out of shape during rebuild and finishing.
How is acoustic recovery verified after repair?
I verify it with calibrated sound measurement, vibration monitoring, baseline comparison, and inspection of contour continuity and surface finish. If the repaired inlet changes tonal output or resonance behavior, the repair is not complete.
Can metal-filled compounds replace weld repair on structural damage?