By the AeroKool Aviation team · Hialeah, Florida
Magnetic particle inspection aircraft parts undergo is a surface and near-surface method: the part is magnetized, and particles gather at the flux leakage a discontinuity creates. It works on ferromagnetic material, and on everything else it is not a method that was rejected on merit. It was never available.
That limit is written into the governing practice. ASTM E1444/E1444M-26, “Standard Practice for Magnetic Particle Testing for Aerospace,” establishes requirements for magnetic particle testing to detect surface or slightly subsurface discontinuities in ferromagnetic materials, and is intended for aerospace applications using the wet fluorescent method. Read the material clause first, before anything about equipment: aluminium is not ferromagnetic, and neither are the austenitic stainless steels common in environmental control system hardware.
So on a large share of component work the first question answers itself, and the useful conversation is about what covers the gap. This article covers how to decide whether the method is a candidate, how the program is built and monitored, how demagnetization is handled, and what the record has to state. The steps are program steps, not bench instructions: every parameter for a specific article comes from the manufacturer’s data and the organization’s approved technique. The methods a component may be inspected with are the wider frame for that choice.
Prerequisites: What Has to Be Settled Before the Part Is Magnetized
- The material. Confirmed ferromagnetic, from the material certification or the manufacturer’s data, not from appearance or from habit.
- The applicable data. The manufacturer’s data for the article, current and accessible as §145.109 requires, since it supplies the technique requirements and the acceptance criteria.
- The written procedure, approved by the authority the quality manual names, with its revision identified and its boundaries stated.
- The material system and process monitoring plan, with the equipment that measures each parameter the procedure depends on.
- The demagnetization decision, made in advance for the article and its next assembly rather than at the end of the shift.
- The authorized readers, qualified by method and level under the organization’s program.
Step 1: Decide Whether the Method Is a Candidate at All
This is the step that saves the most time and is skipped the most often, because a magnetic particle bench in the building creates an assumption that it applies.
confirm the material from the record, not from the part
Ferromagnetic behaviour is a property of the alloy and its condition, and a part’s appearance says very little about it. Establish the material from the certification or from the manufacturer’s data for that part number. On an assembly of mixed materials, the answer differs by piece, which means the inspection plan differs by piece as well.
Two traps sit inside that sentence. The first is the stainless family, which is not one family: some grades are ferromagnetic and the austenitic grades common in thermal and pneumatic hardware are not, so the word stainless on a drawing settles nothing. The second is condition, because processing history can change magnetic behaviour in a way the alloy designation alone does not predict. Where the material is not established from a record, the honest position is that the method’s applicability is unknown rather than assumed.
⚠️ A shop that decides material suitability at the bench, part by part, is making an engineering determination without recording it. The determination belongs in the inspection plan, from the certification or the data, before the article reaches the bench.
decide where magnetic particle inspection aircraft parts cannot go
Where the material rules the method out, the discontinuity of concern does not disappear with it. Surface coverage falls to fluorescent penetrant inspection, and near-surface coverage on conducting non-ferromagnetic material usually falls to eddy current inspection, which is the method that does on aluminium what magnetic particle cannot.
⚠️ Proposing magnetic particle on non-ferromagnetic hardware is one of the most common method-selection errors in component work, and it is visible in a plan long before it wastes a shift.
Step 2: Establish the Technique and Fix It in a Procedure
Magnetization is directional, and a discontinuity is only revealed when the flux crosses it. Everything in the technique follows from that geometry.
make the technique account for orientation and geometry
The procedure has to state how the article is magnetized, in how many directions, and how the sequence covers the features of concern, because a single magnetization direction leaves a whole class of orientations effectively invisible. Geometry drives this: changes in section, holes, keyways, threads and radii all affect where flux goes and where indications will and will not form.
The consequence for planning is that the discontinuity you are looking for has to be named before the technique is chosen. A crack expected at a radius under bending is not oriented like a crack expected along a machined feature, and a technique that suits one may be nearly blind to the other. Where the orientation is genuinely unknown, the answer is coverage in more than one direction rather than confidence in one.
Geometry also produces indications that are real signals about shape rather than about damage. A technique that does not anticipate them leaves the reader to decide, part by part, which indications to take seriously — and that decision, repeated a hundred times without a written basis, is how two inspectors reach two different conclusions about the same feature and both believe they followed the procedure.
state the boundaries of the procedure
Which articles it covers, what happens when a part arrives outside those boundaries, and who answers that question in writing. A procedure with no boundary implies it covers everything, and the first article that falls outside gets processed anyway. What a written NDT procedure has to contain is the requirement behind this step, and whether the shop owns the authority to approve a technique or borrows it decides how quickly the question can be answered.
Step 3: Control the Material System and the Process Monitoring
The practice is written around the wet fluorescent method for aerospace, which means the suspension and the reading conditions are as much part of the measurement as the magnetizing equipment.
scope the monitoring by what drifts
The condition of the particle suspension, the equipment that produces and measures the magnetizing effect, the reading conditions, and the artefact used to verify overall system performance all change over time. Each needs a defined check, and each check needs a recorded value rather than a recorded verdict, because a log of satisfactory tells you nothing until the day it says otherwise.
put every measuring device inside the calibration program
Any device that measures a parameter an airworthiness determination depends on falls under §145.109(b), which requires calibration to a standard acceptable to the FAA. §145.211 makes calibration and its intervals a quality-manual procedure, and what a calibration program has to demonstrate includes the retrospective rule that decides which results are in doubt when one of them is found out of tolerance.
verify the whole system with a controlled artefact
The artefact is the only thing that tells you the combination of equipment, suspension and reading conditions is behaving. It needs individual identification, condition control and a withdrawal rule, and a worn artefact fails in the direction that flatters the shop: it becomes easier to satisfy while real sensitivity falls.
That is also why the system verification has to sit close to the work in time. A check performed at the start of a shift says something about the shift; a check performed monthly says something about the month, and everything processed between two monthly checks shares one unbounded assumption. The frequency is a decision for the procedure, and the reasoning behind it is what an auditor asks for after a check fails.
Detection capability is a property of that whole system rather than of the method, which is the point what a detection result actually proves develops in full. An indication that would have been found on a well-behaved line can be missed on the same line a week later, with no change in the certificate on the wall.
Step 4: Decide Demagnetization Before the Part Is Magnetized
This is where magnetic particle differs from every other method on the list. The inspection changes the state of the article, and that change has consequences downstream.
treat residual magnetism as a condition you introduced
A magnetized part can attract debris in service, and it can interfere with adjacent components, instruments and subsequent measurements. Whether demagnetization is required, how it is verified and what the record says about it are decisions for the manufacturer’s data and the procedure, made before the article is magnetized rather than discovered afterwards.
plan for the assembly the part is going back into
The relevant question is not only whether the part tolerates residual magnetism but whether its next assembly does. On rotating hardware and near sensors and control components, the answer is usually more restrictive than the part alone would suggest.
There is a second-order effect worth planning for as well. A magnetized part interferes with measurements taken on it afterwards, so the order of operations matters: a dimensional check, a balance operation or a subsequent inspection performed on a part still carrying residual magnetism may not be measuring what the operator thinks. Where the process sheet puts magnetic particle in the middle of a sequence rather than at the end, the demagnetization step is not a courtesy to the next owner. It is a precondition for the next operation.
A part that leaves the shop magnetized, with no record of the decision, gives the next organization nothing to work with. It cannot tell whether the condition was evaluated and accepted or simply never considered.
Returning a magnetized article to an assembly that cannot tolerate it converts a clean inspection into an in-service problem, and nothing in the inspection record will point at the cause.
Step 5: Define the Record and the Disposition Route
The record is what makes an inspection reviewable, and the vocabulary in it decides whether the review is a technical conversation or a semantic one.
separate the indication from the verdict
The reader reports what was observed, where, and to what extent. The disposition compares that to the acceptance criteria in the manufacturer’s data for the part number. ASTM E1316-26b is the standard terminology for nondestructive examinations, and it exists precisely so that indication, discontinuity and defect are not used interchangeably in a document where the difference matters.
That distinction is not academic on this method, because magnetic particle produces a category of indication that is genuine, expected and not damage: the signals geometry creates. A record that calls those defects has manufactured a scrap decision, and a record that omits them entirely has hidden the fact that the technique produces them. Reporting what was seen, and separately what it was judged to be, keeps both errors out of the file.
close the chain to the release
§145.213 requires the article to be inspected before it is approved for return to service, requires the inspector making that determination to meet the requirements of §145.155, and restricts the maintenance release signature, inside the United States, to an employee appropriately certificated as a mechanic or repairman under part 65. The method authority and the signature authority are separate grants, and the records the finding has to leave behind are what connect them.
Common Magnetic Particle Problems and How to Trace Them
- No indications on a part with a known service history. Check the material first: the method may never have applied. Then check the magnetization directions against the orientations of concern.
- Indications clustered at geometric features. Trace the technique before the metallurgy: section changes, holes and radii concentrate flux and produce non-relevant indications by design.
- Indications that disappear on reprocessing. Trace the suspension condition and the reading conditions, in that order.
- A part that arrives already magnetized. Establish where it came from, because the previous process may have introduced a condition that affects both this inspection and the assembly.
- Demagnetization performed and unverified. The verification and its record are the only evidence, and their absence is the finding.
- A monitoring check failed with no impact assessment. That is the calibration program’s retrospective rule, absent.
- Acceptance criteria quoted from the ASTM practice. The practice establishes requirements for the method; the criteria for the article come from the manufacturer’s data.
- Non-ferromagnetic parts on the inspection plan. Trace how the plan was built, because the same assumption is probably elsewhere in it.
Warning Signs of a Minimum-Standard Approach
- Material confirmation taken from appearance or from the part’s family rather than from a record.
- A single magnetization direction for articles with discontinuities of unknown orientation.
- Monitoring limited to the magnetizing equipment, with the suspension unmonitored.
- No individually identified reference artefact, or one with no condition history.
- Demagnetization treated as an optional final step with no decision recorded.
- Personnel authorized for NDT generically rather than for this method at a level.
- Records that state the method and a pass, with no location or extent.
- A procedure with no revision, no approval signature and no stated boundaries.
Expected Outcome: A Result That Says What Was Actually Examined
A defensible magnetic particle program produces a record a stranger can reconstruct: the material and how it was confirmed, the procedure and revision applied, the magnetization sequence, the suspension and its monitoring, the artefact used to verify the system, the equipment identified individually, the reader and the authorization behind them, the indication as observed with its location and extent, the disposition against a named data revision, and the demagnetization decision with its verification.
With that record, a later inspection of the same part is comparable to this one. Without it, the second inspection starts from nothing and the two results cannot be reconciled, which is how a component acquires a history nobody trusts.
The commercial value of that record shows up in the argument nobody plans for. When an article comes back with a discontinuity in a location that was inspected, the question is whether the method could have found it at the size it then was — and the only way to have that conversation as engineering rather than as blame is to have written down what was examined, in which directions, under what verified system, against which data revision.
Frequently Asked Questions
what materials can magnetic particle inspection be used on?
Ferromagnetic materials. ASTM E1444/E1444M-26 establishes requirements for detecting surface or slightly subsurface discontinuities in ferromagnetic material, intended for aerospace applications using the wet fluorescent method. Aluminium and austenitic stainless steels are not ferromagnetic, so the method does not apply to a large share of environmental control system hardware.
how deep can magnetic particle inspection detect?
The method addresses discontinuities at the surface and slightly below it. It is not a volumetric method, so anything deeper in the section requires ultrasonic or radiographic coverage, and the depth that counts as slightly subsurface for a specific article depends on the technique and the manufacturer’s data rather than on a general figure.
does a part have to be demagnetized after inspection?
That depends on the manufacturer’s data, the article and the assembly it returns to. Residual magnetism can attract debris and interfere with adjacent components and instruments, so the decision, the method of demagnetization and its verification belong in the procedure and the record rather than in shop practice.
what is the difference between magnetic particle and penetrant inspection?
Physics and reach. Penetrant reveals discontinuities open to the surface on nonporous materials of any kind. Magnetic particle reveals surface and slightly subsurface discontinuities, and only on ferromagnetic material. On aluminium hardware penetrant and eddy current do the work magnetic particle cannot.
who sets the acceptance criteria for a magnetic particle indication?
The approved data for the part number: the component maintenance manual, the overhaul manual, the service bulletin or the repair data the organization is approved to use. The ASTM practice establishes requirements for performing the examination, not the criteria for accepting a specific article.
what qualification do magnetic particle inspectors need?
Qualification under the employer’s own program, by method and level. AC 65-31B states that in the United States there is no national certification requirement or standard to determine that NDI personnel are qualified, so the standard adopted, the level and the certifying party have to be asked about specifically.
Ask the material question before the equipment question, and plan the magnetization for the orientations you cannot see. Where the alloy rules the method out, say so in the plan rather than running the part anyway, because a clean result from a method that never applied is worse than no result at all.
About AeroKool Aviation. AeroKool Aviation is an FAA-certificated repair station in Hialeah, Florida, specializing in the repair and overhaul of environmental control system components — air cycle machines, cooling turbines, heat exchangers, refrigeration packages, valves and environmental control units — for commercial, regional, business jet, rotorcraft and military operators. The company was founded in 1959 and holds AS9110C and AS9100D registrations, with in-house PMA parts manufacturing and FAA DER repair engineering. Component capability is organized by aircraft category, manufacturer, model and component type in the component capability listing, down to individual part numbers such as this valve for a legacy regional platform.
This article is general technical information about magnetic particle inspection programs for aircraft components. It is not approved data, it is not a maintenance procedure, and it does not replace the component maintenance manual, structural repair manual, service bulletin, airworthiness directive or other airworthiness data your organization is approved to use. Standards, advisory material and manufacturer data are revised, and the techniques, parameters and acceptance criteria that apply to a specific inspection depend on the part number, the material, the geometry and the scope of the repair station’s certificate. Verify the applicable requirements against the current manufacturer data, your own quality control manual and its written procedures, and your principal inspector or Level III authority before performing or accepting any inspection.
Talk to AeroKool Aviation
AeroKool Aviation is an FAA-certificated repair station in Hialeah, Florida, overhauling air cycle machines, cooling turbines, heat exchangers, valves and environmental control units for commercial, regional, business and military operators since 1959, with an AS9110C quality system and in-house PMA and DER engineering. If you have a component on the bench, a repeat removal you cannot explain, or a part number you cannot source, we will tell you what falls inside our ratings and what does not. Request a quote with the part number and the condition you need resolved, and the answer will name the scope it falls under.
Address
1495 S.E. 10th Avenue Hialeah, FL 33010-5984
eMail
aerokool@aerokool.com | sales@aerokool.com
Phone
305.887.6912 | 800.458.4255